Research Article
Comparing the effect of a desensitizing material and a self-etch adhesive on dentin sensitivity after periodontal surgery: a randomized clinical trial
Hila Hajizadeh, Atefeh Nemati-Karimooy, Sara Majidinia, Amir Moeintaghavi, Marjaneh Ghavamnasiri
Restor Dent Endod 2017;42(3):168-175.   Published online July 21, 2017
DOI: https://doi.org/10.5395/rde.2017.42.3.168
AbstractAbstract PDFPubReaderePub
Objectives

This double-blind randomized placebo-controlled clinical trial evaluated the ability of a desensitizing agent and a self-etch adhesive on cervical dentin sensitivity (CDS) after periodontal surgery.

Materials and Methods

Ninety hypersensitive teeth of 13 subjects were included in the study. After periodontal surgery, the teeth of each posterior sextant treated with one of the following materials: G1: Clearfil S3 Bond (Kuraray Dental), G2: Gluma Desensitizer (Heraeus Kulzer), and G3: placebo (water). The sensitivity was assessed using evaporative stimuli before treatment (baseline, T0), 1 day after treatment (T1), after 1 week (T2), and after 1 month (T3) according to visual analog scale (VAS).

Results

Following the treatment, all the 3 groups showed significant reduction of CDS in T1 compared to T0. Reduction of CDS between T1 and T2 was observed only in G1 but there was no significant difference between T2 and T3 in this group. Although we observed a significant difference in T3 compared to T1 and T2 in G2 and G3, comparison of treatment groups in each assessment time showed a significant difference only in T3. According to paired comparison, this was due to the difference between G2 and G3.

Conclusions

Dentin sensitivity following periodontal surgery will decrease spontaneously over time, but treating the sensitive teeth with Gluma Desensitizer and Clearfil S3 Bond can have some benefits.

  • 28 View
  • 0 Download
Close layer
Original Article
Effect of rewetting agent on dentinal microtensile bond strength
Hee-Young Kang, Young-Gon Cho, Jong-Uk Kim, Byung-Cheul Park, Sang-Hoon Yoo, Cheul-Hee Jin, Hee-Young Choi, Young-Jae Ki
J Korean Acad Conserv Dent 2004;29(2):153-161.   Published online March 31, 2004
DOI: https://doi.org/10.5395/JKACD.2004.29.2.153
AbstractAbstract PDFPubReaderePub

This study investigated that the effect of rewetting agent on dentinal microtensile bond strength (µTBS). Human molars were sectioned to expose the superficial dentin surfaces.

Samples were divided into two groups according to type of adhesives-Single Bond (S) and One-Step (O)], and again subdivided into five groups by different dentin surface treatment-dry for 15s (D), blot dry (BD) or dry for 15s, and rewet with different rewetting agents [distilled water (DW), Gluma Desensitizer (GD) and Aqua-Prep (AP)] for 30s. After application of adhesive, composite resin was built up on the bonding surface. Each tooth was sectioned to obtain stick with 1 mm2 cross sectional area and the µTBS was determined by EZ test.

In the S group, the mean µTBS of GD, AP and BD group was significantly higher than that of DW and D group (p < 0.05). In the O group, the mean µTBS of AP, GD, BD and DW group was significantly higher than that of D group (p < 0.05).

The data suggested that Gluma Desensitizer and Aqua-Prep could be successfully used as rewetting agents, and Distilled water could be acceptable in aceton based adhesive system only.